The textbooks in this acclaimed series introduce the nonspecialist to the fundamentals and recent developments of a particular field. The current volume focuses on Auger electron spectroscopy and X-ray photoelectron spectroscopy, with an emphasis on current applications. Physicists, chemists, and materials scientists will learn principles of operation, some design theory, and assessment techniques.